• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Dissertação de Mestrado
DOI
https://doi.org/10.11606/D.85.2011.tde-26012012-145626
Documento
Autor
Nome completo
Patricia Brissi Santos
E-mail
Unidade da USP
Área do Conhecimento
Data de Defesa
Imprenta
São Paulo, 2011
Orientador
Banca examinadora
Takiishi, Hidetoshi (Presidente)
Genova, Luís Antonio
Périgo, Elio Alberto
Título em português
Efeitos da adição de surfactante e moagem de alta velocidade  em pós magnéticos à base de Pr-Fe-B obtidos via HDDR
Palavras-chave em português
ímãs permanentes
liga Pr-Fe-Co-B
pós magnéticos
surfactante
Resumo em português
Esse trabalho teve como objetivo verificar o efeito da adição do ácido oléico na moagem de alta velocidade/energia na obtenção de pós magnéticos em escala nanométricas da liga Pr12Fe65,9Co16B6Nb0,1. A primeira etapa deste trabalho, envolveu a obtenção de pós magnéticos por meio do processo de hidrogenação, desproporção, dessorção e recombinação (HDDR), utilizando a pressão de H2 de 930 mbar (hidrogenação e desproporção) e temperatura de dessorção e recombinação de 840 ºC. Inicialmente, os pós HDDR foram submetidos à moagem de alta velocidade/energia a 900 rpm, com variação do volume do meio de moagem (ciclohexano) sem adição de ácido oleico. Em seguida, os pós HDDR foram submetidos à moagem com adição de ácido oleico, variando o tempo de moagem. Após a moagem, foi realizado tratamento térmico dos pós a 700 ºC ou 800 ºC durante 30 min., com a finalidade de cristalização do pó. Foi verificado que, a utilização de 6,6 ml de ciclohexano como meio de moagem e com adição de ácido oleico há uma melhora na eficiência da moagem dos pós. Para adições de surfactante, de 0,02 a 0,05 ml e tempos de moagem até 360 minutos, não ocorre a aglomeração dos pós magnéticos no pote de moagem, obtendo acima de 90% de eficiência na moagem. A segunda etapa deste trabalho envolveu a caracterização dos pós magnéticos: utilizando magnetômetro de amostra vibrante, microscopia eletrônica de Varredura, microscopia eletrônica de transmissão e difração de raios-X. Os resultados obtidos mostraram que a adição de ácido oléico na moagem de alta velocidade/energia proporciona uma melhora nas propriedades magnéticas. Com a variação do tempo de moagem a fase Fe-α presente no pó HDDR apresenta diminuição no tamanho do cristalito (de 35 para ~ 10 nm) enquanto que, na fase Pr2Fe14B verifica-se menor grau de cristalinidade.
Título em inglês
Effects of surfactant addition and high-speed ball milling on magnetic powders based on Pr-Fe-B obtained by HDDR
Palavras-chave em inglês
magnetic powders
permanent bonded magnets
Pr-Fe-Co-B alloy
surfactant
Resumo em inglês
This work verified the effect caused by adding the surfactant in the high speed/energy milling in order to obtain Pr12Fe65.9Co16B6Nb0.1 magnetic nanopowders. The first part of this work involved the magnetic powder obtainment through the process of hydrogenation, disproportionation, desorption and recombination (HDDR). The pressure of H2 during the hydrogenation and disproportion steps was 930 mbar and the temperature of desorption and recombination was 840 ºC. Initially, the HDDR powders were subjected a highspeed milling process at 900 rpm, with quantity variations of the milling medium (cyclohexane) and without the addition of oleic acid. Then, the HDDR powders were subjected to the milling process with the addition of oleic acid and with milling time variations. After the milling process, heat treatments of the powder were carried out at 700 °C or 800 °C for 30 minutes in order to obtain the crystallization of the powder. By performing the procedures, it was verified that the milling efficiency improved with the addition of 6.6 ml of cyclohexane as the milling medium and with the addition of oleic acid. It was determined that for the surfactant additions of 0.02 ml to 0.05 ml, with a milling time of up to 360 minutes, powder agglomeration does not occur in the milling pot and the milling efficiency is higher than 90%. The second stage of this work involved the magnetic powders characterization obtained by using vibrating sample magnetometer, scanning electron microscopy, transmission electron microscopy and X-ray diffraction. Through the characterizations it was found that the powders magnetic properties improved when the addition of oleic acid in a high-speed /energy milling occurred. It was also verified that the α-Fe phase, present in the powder, shows a crystallite size decrease (from 35 nm to ~ 10 nm) when the time milling variation occurred; meanwhile, the crystallinity degree was lower in the Pr2Fe14B phase when the time milling variations was carried out.
 
AVISO - A consulta a este documento fica condicionada na aceitação das seguintes condições de uso:
Este trabalho é somente para uso privado de atividades de pesquisa e ensino. Não é autorizada sua reprodução para quaisquer fins lucrativos. Esta reserva de direitos abrange a todos os dados do documento bem como seu conteúdo. Na utilização ou citação de partes do documento é obrigatório mencionar nome da pessoa autora do trabalho.
2011SantosEfeitos.pdf (5.30 Mbytes)
Data de Publicação
2012-01-30
 
AVISO: Saiba o que são os trabalhos decorrentes clicando aqui.
Todos os direitos da tese/dissertação são de seus autores
CeTI-SC/STI
Biblioteca Digital de Teses e Dissertações da USP. Copyright © 2001-2024. Todos os direitos reservados.