• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.85.2023.tde-28122023-102054
Documento
Autor
Nombre completo
Marcela Enaile de Melo Faria
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Paulo, 2023
Director
Tribunal
Martinez, Luis Gallego (Presidente)
Bock, Eduardo Guy Perpétuo
Silva, Suelanny Carvalho da
Título en portugués
Influência do disprósio nas propriedades magnéticas dos ímãs permanentes à base de NdFeB obtidos por HD
Palabras clave en portugués
ímãs de NdFeB
ligas magnéticas
variação de Dy
variações de processamento
Resumen en portugués
Os ímãs de terras-raras mostraram-se importantes no desenvolvimento de dispositivos eletromagnéticos. Embora estes ímãs tenham promovido avanços, a baixa temperatura de Curie impede a utilização em altas temperaturas. Sabe-se que a adição de disprósio melhora as propriedades magnéticas, controla o tamanho do grão e aumenta a temperatura de trabalho. As pesquisas atuais focam em diminuir a quantidade de disprósio utilizada nos ímãs. Uma liga rica em disprósio foi produzida no Instituto de Pesquisa Tecnológica (IPT) para ser usada como aditivo nas ligas magnéticas (Nd14,1B6,1Febal e Nd8,7Dy4,9B6,1Febal), adquiridas com a Less Common Metal Ltd. Entretanto essas últimas ligas ao passarem por uma análise de raios X, constatou-se que havia a presença de ferro livre, que é deletério para as propriedades magnéticas. Foi necessário realizar tratamento térmico para que o Fe-α pudesse ser eliminado. O presente trabalho analisa a influência da variação do disprósio dentro dos ímãs (0%, 10%, 20% e 30%) e avalia a variação de outros parâmetros de processamentos, como: tempo de tratamento térmico (TT) (sem tratamento, 2,5h e 5h) e o tempo de moagem (45 min, 53 min e 60 min). As variações realizadas tinham o objetivo de verificar qual resultaria em tamanhos de grãos favoráveis para a sinterização e nas propriedades magnéticas. Melhores resultados foram obtidos com TT de 5h, moída por 60 min e com 10% de massa de Dy; obteve-se iHc = 736 k.A.m-1, Jr = 1,18 T e BHmax = 4,32 kJm-3.
Título en inglés
Dysprosium influence on magnetic properties of NdFeB-based permanent magnets obtained by HD
Palabras clave en inglés
Dy variation
magnetic alloys
NdFeB magnets
parameters variation
Resumen en inglés
The rare-earth magnets were showed important in the development of electromagnetic devices. However, these magnets had promoted advances, the low Curie temperature prevent its usage in high temperatures. It's known that the dysprosium addition improves the magnetic properties, control the grain size, and raise the working temperature. The current research focus on minimizing the quantity of dysprosium used in the magnets. A rich dysprosium alloy was produced in the Technological Institute Research (IPT) to be used as additive in the magnetic alloys (Nd14,1B6,1Febal and Nd8,7Dy4,9B6,1Febal), acquired with Less Common Metal Ltd. Although these alloys after an X-ray analyzes, was determined the presence of free iron, that's deleterious for the magnetic properties. It was necessary to realize a heat treatment to eliminate the Fe-α. This present dissertation analyzes the influence of dysprosium variation within the magnets (0%, 10%, 20% e 30%) and evaluate the variation of processing parameters, like the time of the heat treatment (without heat treatment, 2.5h and 5h) and the milling time (45 min, 53 min and 60 min). The variation had the object to investigate which variation would provide better grain sizes for the sinterization and the magnetic properties. Better results were obtained for heat treatment of 5h, milled for 60 min and 10%w of Dy; obtained iHc = 736 k.A.m-1, Jr = 1.18 T and BHmax = 4.32 k.J.m-3.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2024-01-08
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.