Dissertação de Mestrado
DOI
https://doi.org/10.11606/D.85.2022.tde-28122023-095246
Documento
Autor
Nome completo
Ivan Douglas Campos
E-mail
Unidade da USP
Área do Conhecimento
Data de Defesa
Imprenta
São Paulo, 2022
Orientador
Banca examinadora
Parra, Duclerc Fernandes (Presidente)
Bonse, Baltus Cornelius
Fermino, Danilo Marin
Título em português
Estudo de compósitos de poli (ácido lático) com celulose extraída da coroa do abacaxi
Palavras-chave em português
comportamento térmico
ensaios
fibra de abacaxi
PLA
Resumo em português
A incessante busca pela redução de poluentes no mundo, principalmente os oriundos dos plásticos sintéticos, faz com que muitos pesquisadores recorram a pesquisas de materiais alternativos. Neste estudo, foram preparados 5 Compósitos de PLA contendo 0,5%, 1,0%, 1,5%, 5% e 10% de fibra de abacaxi. Foram ensaiadas a partir do PLA puro e PLA com adição de fibras, sem acréscimo de nenhum estabilizante ou qualquer outro material nas amostras com 0,5%, 1,0% e 1,5%, com foco na estratégia de verificação do comportamento do PLA com a fibra considerando como referência o PLA puro e as amostras com 5,0% e 10,0% foram adicionadas de compatibilizante Polybond. As fibras foram trituradas e incorporadas no PLA no estado fundido por meio de um moinho de facas e, em seguida, as formulações foram homogeneizadas em uma extrusora dupla rosca. Os corpos de prova foram obtidos em uma prensa a 180ºC e em seguida cortados com gabarito. A caracterização das amostras foi realizada por meio das técnicas de ensaios mecânicos, Calorimetria Diferencial Exploratória (DSC), Termogravimetria (TGA), Espectroscopia no Infravermelho por Transformada de Fourier (FT-IR) e Microscopia Eletrônica de Varredura (MEV). O comportamento do compósito trouxe uma alteração na dureza a partir da adição de fibras no PLA, em torno de 3,8% na amostra PLA + 0,5% Fibra; 8,9% na amostra PLA + 1,0% Fibra; 6,2% na amostra PLA + 1,5% Fibra;13,5% na amostra PLA + 5% Fibra e 6,5% na amostra PLA + 10% Fibra. Quanto ao impacto, o compósito PLA + fibra apresentou um ganho em sua resistência. A matriz com adição de fibras, apresentou uma melhora na resistência à tração. Quanto ao comportamento térmico, observa-se que os compósitos com fibra não apresentam alterações de estabilidade térmica, permanecendo assim, na mesma faixa de degradação do polímero puro e da fibra.
Título em inglês
Study of poly (lactic acid) composites with cellulose extracted from the pineapple crown
Palavras-chave em inglês
pineapple fiber
PLA
testing
thermal behavior
Resumo em inglês
The relentless demand for the reduction of pollutants in the world, especially those from synthetic plastics, makes many researchers turn to the investigation of alternative materials. In this study, 5 PLA composites containing 0.5%, 1.0%, 1.5%, 5% and 10% pineapple fiber were prepared. The samples with 0.5%, 1.0% and 1.5% were tested from pure PLA and PLA with fibers added, without adding any stabilizer or any other material, focusing on the strategy of verifying the behavior of PLA with the fiber considering pure PLA as reference, and the samples with 5.0% and 10.0% were added the compatibilizer polybond. The fibers were ground and incorporated into the PLA in the molten state using a knife mill, and then the formulations were homogenized in a twin-screw extruder. The samples were obtained in a press at 180ºC and then cut using a die. Characterization of the samples was done by mechanical testing, Differential Scanning Calorimetry (DSC), Thermogravimetry (TGA), Fourier Transform Infrared Spectroscopy (FT-IR) and Scanning Electron Microscopy (SEM). The behavior of the composite brought a change in the hardness of the addition of fibers in PLA, about 3.8% in the sample PLA + 0.5% Fiber; 8.9% in the sample PLA + 1.0% Fiber; 6.2% in the sample PLA + 1.5% Fiber;13.5% in the sample PLA + 5% Fiber and 6.5% in the sample PLA + 10% Fiber. As for impact, the composite PLA + fiber presented a gain in its resistance. The matrix with fiber addition, presented an improvement in tensile strength. Regarding thermal behavior, it is observed that composites with fiber do not present changes in thermal stability, thus remaining in the same degradation range as the pure polymer and fiber.
 
AVISO - A consulta a este documento fica condicionada na aceitação das seguintes condições de uso:
Este trabalho é somente para uso privado de atividades de pesquisa e ensino. Não é autorizada sua reprodução para quaisquer fins lucrativos. Esta reserva de direitos abrange a todos os dados do documento bem como seu conteúdo. Na utilização ou citação de partes do documento é obrigatório mencionar nome da pessoa autora do trabalho.
2022CamposEstudo.pdf (3.67 Mbytes)
Data de Publicação
2024-01-08
 
AVISO: Saiba o que são os trabalhos decorrentes clicando aqui.
Todos os direitos da tese/dissertação são de seus autores
CeTI-SC/STI
Biblioteca Digital de Teses e Dissertações da USP. Copyright © 2001-2024. Todos os direitos reservados.