Tesis Doctoral
DOI
https://doi.org/10.11606/T.85.2016.tde-23052016-092648
Documento
Autor
Nombre completo
Eliner Affonso Ferreira
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Paulo, 2013
Director
Tribunal
Faria Júnior, Rubens Nunes de (Presidente)
Ett, Gerhard
Lazar, Dolores Ribeiro Ricci
Marcondes, Paulo Victor Prestes
Politano, Rodolfo
Título en portugués
Estudo da hidrogenação para pulverização de ligas à base de terras raras com Nb para eletrodos de hidreto metálico
Palabras clave en portugués
baterias
eletrodos
hidreto
nióbio
níquel
Resumen en portugués
Neste trabalho foram estudadas as series de ligas La0,7Mg0,3Al0,3Mn0,4Co(0,5-x)NbxNi3,8 (x =0 a 0,5) e La0,7Mg0,3Al0,3Mn0,4Nb(0,5-x)Ni(3,8-x) (x =0,3; 0,5 e 1,3), como eletrodo negativo de baterias de Níquel Hidreto Metálico. A pulverização das ligas foi realizada com duas pressões de H2 (2 bar e 9 bar). A capacidade de descarga das baterias de níquel hidreto metálico foi analisada pelo equipamento de testes elétricos Arbin BT-4. As ligas, no estado bruto de fusão, foram analisadas por microscopia eletrônica de varredura (MEV), espectroscopia de energia dispersiva (EDS) e difração de raios-X. Com o aumento da concentração de nióbio nas ligas nota-se a diminuição da estabilidade cíclica das baterias e da capacidade máxima de descarga. A capacidade de descarga máxima obtida foi para a liga La0,7Mg0,3Al0,3Mn0,4Co0,5Ni3,8 (45,36 mAh) e a bateria que apresentou a melhor performance foi a liga La0,7Mg0,3Al0,3Mn0,4Co0,4Nb0,1Ni3,8 (44,94 mAh).
Título en inglés
Study of hydrogenation for pulverization of rare earth alloys with nb for metal hydride electrodes
Palabras clave en inglés
battery
electrode
hydride
nickel
niobium
Resumen en inglés
In this work were studied La.7Mg0.3Al0.3Mn0,4Co(0.5-x)NbxNi3.8 (x= 0 - 0.5) and La0,7Mg0,3Al0,3Mn0.4Nb(05+x)Co0,5Ni(3.8-x). (x=0.3; 0.5;1.3) alloys for negative electrodes of the Nickel-Metal Hydride batteries. The hydrogenation of the alloys was performed varying pressing of H2 (2 and 9 bar). The discharge capacity of the nickel-metal hydride batteries were analyzed in the Arbin BT-4 electrical test equipment. The as-cast alloys were analyzed by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDX) and X-Ray diffraction. The increasing Niobium addition in the alloys decreased cycle life and the maximum discharge capacity of the batteries. The maximum discharge capacity was obtained with the La.7Mg0.3Al0.3Mn0,4Co0.5Ni3.8 (45.36 mAh) and the battery which presented the best performance was La.7Mg0.3Al0.3Mn0.4Co0.5Nb0.1Ni3.8 (44.94 mAh).
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2016-06-06
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.