Nombre completo
Deborah Yohana Bertoldo da Silva
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Paulo, 2023
Director
Tribunal
Muccillo, Eliana Navarro dos Santos (Presidente)
Reis, Shirley Leite dos
Toffoli, Samuel Marcio
Título en portugués
Propriedades dielétricas da titânia co-dopada
Palabras clave en portugués
dopantes
microestrutura
propriedades dielétricas
titânia
Resumen en portugués

Neste trabalho foram investigadas a microestrutura, as propriedades elétricas e dielétricas da titânia contendo dopantes à base de terras raras. O principal objetivo foi avaliar o efeito da temperatura de sinterização e da concentração de dopantes tri- e pentavalentes na microestrutura e nas propriedades elétricas e dielétricas dos materiais sinterizados. Cerâmicas de TiO2 contendo Y2O3 e Nb2O5 foram preparadas pelo método convencional de mistura dos reagentes na proporção estequiométrica seguida de reação em altas temperaturas. Os teores de dopantes foram de 2,5; 5 e 10% mol e as temperaturas de sinterização foram 1480 e 1500 ºC. A caracterização das amostras foi realizada por meio de técnicas de difração de raios X, para identificação das fases cristalinas, e observação da microestrutura em microscópio eletrônico de varredura com espectroscopia de energia dispersiva associada e microscopia de varredura por sonda. As propriedades elétricas e dielétricas foram estudadas por meio de medidas de espectroscopia de impedância. A microestrutura resultante evidenciou a formação de fases de impureza, especialmente YNbTiO6, para 5% e 10% mol de dopantes, e densidades aparentes acima de 80% da densidade teórica. Além da fase de impureza, excesso de dopantes deram origem a outras fases nos contornos de grão, como evidenciado por microscopia eletrônica. Os tamanhos médios de grão variaram entre 20 e 30 µm. A sinterização em 1500 ºC produziu uma fase amorfa nos contornos de grão e crescimento acentuado dos mesmos, sugerindo a formação de fase líquida durante a sinterização. Para todas as composições foi obtida permissividade elétrica colossal (acima de 1.000). Valores de energia de ativação para a condução através dos contornos de grão variaram entre aproximadamente 0,2 e 0,33 eV evidenciando um comportamento semicondutor. A tangente de perdas a 60 ºC foi de ≈ 0,2. A maior permissividade elétrica foi obtida para a composição contendo 5% mol de dopantes.

Título en inglés
Dielectric properties of co-doped titania
Palabras clave en inglés
dielectric properties
dopants
microstructure
titania
Resumen en inglés

In this work, the microstructure, the electrical and dielectric properties of titania containing rare earth co-dopants were investigated. The main purpose was to evaluate the effect of the sintering temperature and the tri-and pentavalent co-dopants on the microstructure and the electrical and dielectric properties of sintered materials. TiO2 ceramics containing Y2O3 and Nb2O5 were prepared by the conventional method of mixture of the starting reagents followed by reaction at high temperatures. Total dopant contents were 2.5, 5 and 10 mol%, and the sintering temperatures were 1480 and 1500 ºC. The sintered specimens were analyzed by Xray diffraction for phase characterization, and microstructure observation by scanning electron microscopy coupled with energy dispersive spectroscopy and scanning probe microscopy. The electric and dielectric properties were studied by impedance spectroscopy measurements. The final microstructure revealed impurity phases, especially YNbTiO6 for 10 mol% total dopants, and apparent densities above 80% of the theoretical value. Besides that, impurity phase, excess dopants gave rise to other impurity phases along the grain boundaries, as evidenced by electron microscopy. The estimated mean grain size was 20-30 µm. For specimens sintered at 1500 ºC, an amorphous phase was detected at the grain boundaries along with sharp increase of the grain size, suggesting liquid phase formation during sintering. Colossal electric permittivity (above 1,000) was obtained for all compositions. Activation energy values for conduction along the grain boundaries varied from 0.2 to 0.33 eV evidencing a semiconducting behavior. The loss tangent at 60 ºC was ≈ 0.2. The highest electric permittivity was obtained for 5 mol% total dopants.

 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2023-06-13
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.