• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.18.2020.tde-04092020-145939
Documento
Autor
Nombre completo
Camila Aguiar Teixeira
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Carlos, 2020
Director
Tribunal
Oliveira, Marcelo Falcão de (Presidente)
Coury, Francisco Gil
Gargarella, Piter
Título en portugués
Microestrutura e resistência à flexão da liga Vitreloy® 106A com diferentes teores de oxigênio e microadição de ítrio
Palabras clave en portugués
ensaio de flexão
fratura
ítrio
oxigênio
vidros metálicos maciços
Resumen en portugués
Os vidros metálicos maciços (VMMs) à base de zircônio se destacam por exibirem elevada tendência à formação vítrea (TFV), alta estabilidade térmica e excelentes propriedades mecânicas. No entanto, a contaminação por oxigênio afeta de maneira significativa tanto sua TFV quanto suas propriedades mecânicas. A presença de oxigênio favorece o mecanismo de cristalização e, quando em solução na matriz, causa fragilização da mesma. A presente dissertação de mestrado avaliou a influência de diferentes teores de oxigênio, 150 a 2000 ppm (parte por milhão em peso), na TFV e propriedades mecânicas, por ensaio de flexão, do VMM Vitreloy® 106a (Vit 106a). Além disso, com o objetivo de reduzir os efeitos negativos do oxigênio, estudou-se influência da adição de ítrio (estequiométrico ao teor de oxigênio de 1000 ppm) na TFV e no comportamento mecânico da Vit 106a quando submetida à flexão. As análises microestruturais revelaram um aumento da fração cristalina com o aumento do teor de oxigênio. O padrão de difração apontou a presença da conhecida fase "big cube" para as amostras com 900, 1000 e 2000 ppm. Ensaios de flexão exibiram uma redução de resistência à fratura e ductilidade, e, para teores maiores que 900 ppm, a deformação plástica foi imperceptível. Análises da superfície de fratura sugerem que a presença de oxigênio desestabiliza o processo de deformação plástica da Vit 106a e os cristais formados, possivelmente contribuem para acelerar o processo de fratura catastrófica. Para a amostra dopada com ítrio, as análises microestruturais e padrão de difração revelaram a formação exclusiva de óxido de ítrio, assim como, uma melhora da TFV da liga. Ensaios de flexão mostraram uma significativa melhora na resistência à fratura e certa deformação plástica. Análises da superfície de fratura sugerem que a adição de ítrio ajudou na estabilização do processo de cisalhamento da banda de principal e o óxido de ítrio parece também atuar como obstáculo para sua propagação.
Título en inglés
Microstructure and bending resistance of the Vitreloy® 106a with different oxygen contents and microaddition of yttrium
Palabras clave en inglés
bending test
bulk metallic glass
fracture
oxygen
yttrium
Resumen en inglés
The zirconium-based bulk metallic glasses (BMGs) stand out due to their high glass forming ability (GFA), high thermal stability and excellent mechanical properties. However, oxygen contamination can significantly affect their GFA and mechanical properties. Oxygen presence can favor the crystallization mechanism and, when in solution in the amorphous matrix, causes embrittlement. The present work evaluated the influence of different oxygen concentrations, from 150 to 2000 ppm (part per million by weight), on the GFA and mechanical properties, by bending test, of the BMG Vitreloy® 106a (Vit 106a). In addition to that, aiming to reduce the oxygen negative effect, it was studied the addition of yttrium (stoichiometric to the oxygen content – 1000 ppm) on the GFA and mechanical behavior of the Vit 106a when submitted to bending tests. The microstructural analyses of the samples contaminated with different oxygen contents have revealed an increase of crystalline fraction following oxygen increment. The diffraction patterns have shown the presence of the known big cube phase for samples contaminated with 900, 1000 and 2000 ppm of oxygen. Bending tests have shown a fracture resistance and ductility reduction, and, for samples with more than 900 ppm of oxygen, plastic deformation was imperceptible. Fracture surface analyses have suggested that the presence of oxygen destabilize the Vit 106a plastic deformation process and the crystals formed, possibly contribute to accelerate the catastrophic fracture process. For samples with yttrium, microstructural analyses and diffraction pattern have revealed the yttrium oxide exclusive formation, as well as, a GFA enhancement. Bending tests have shown a significative fracture resistance improvement and some plastic deformation. Fracture surface analyses have suggested that yttrium addition aided the shear banding process stabilization and the yttrium oxide appeared also to drag the main shear band propagation.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2021-06-28
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.