• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Mémoire de Maîtrise
DOI
https://doi.org/10.11606/D.18.2005.tde-24012008-111028
Document
Auteur
Nom complet
Shirley Minnell Ferreira de Oliveira
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Carlos, 2005
Directeur
Jury
Parreira, Alexandre Benetti (Président)
Fernandes Junior, José Leomar
Trichês, Glicério
Titre en portugais
Estudo do comportamento mecânico de misturas de fosfogesso e cal para utilização na construção rodoviária
Mots-clés en portugais
Fosfogesso
Misturas estabilizadas com cal
Pavimento
Reciclagem
Resumé en portugais
Este trabalho tem como objetivo estudar, a partir de ensaios de laboratório, o comportamento mecânico de misturas de fosfogesso e cal destinadas à construções de bases e sub-bases rodoviárias. O fosfogesso é um resíduo resultante da produção do ácido fosfórico, principal componente de fertilizantes fosfatados. O fosfogesso é gerado em grande escala, originando sérios problemas de armazenagem. Restrições de leis ambientais e o aumento do custo de espaço para a armazenagem do fosfogesso têm estimulado pesquisas para a aplicação desse material. Entre as pesquisas, encontra-se, o aproveitamento desse resíduo como material de construção de bases e sub-bases rodoviárias. As amostras destas misturas foram submetidas a ensaios de compressão simples, compressão diametral e CBR. Nos ensaios de compressão simples e compressão diametral, os corpos de prova foram ensaiados sem imersão e após imersão prévia em água por quatro horas. Para todos os teores de cal utilizados (0%, 3%, 5%, 7% e 10%) os corpos-de-prova foram compactados na energia equivalente ao Proctor modificado. Para cada teor de cal os corpos-de-prova passaram por processo de cura de 0, 3, 7 e 28 dias. Quatro réplicas foram moldadas para cada condição de ensaio, obtendo-se a média dos resultados pelo método estatístico de GRUBBS. Concluiu-se com esses ensaios que valores crescentes de tempo de cura e de teor de cal conduziram a maiores valores de resistência e de rigidez. Além disso, ensaios realizados após a imersão em água apresentaram valores de resistência à compressão simples, resistência à compressão diametral e rigidez menores do que os obtidos sem imersão. Observou-se também que as misturas de fosfogesso e cal, no geral, apresentaram melhores resultados de resistência à compressão simples, resistência à compressão diametral e coesão do que as misturas de solo cal. Entretanto as misturas compostas por fosfogesso e cimento obtiveram valores superiores de resistência e rigidez se comparada com as misturas de fosfogesso e cal.
Titre en anglais
Mechanical behavior study of mixtures of phosphogypsum and lime to road construction utilization
Mots-clés en anglais
Lime-treated mixtures
Pavement
Phosphogypsum
Recycling
Resumé en anglais
This work has the aim of study, considering laboratory experiments, the mechanical behavior of a mixture of phosphogypsum and lime to be used in bases and sub-bases of road construction. The phosphogypsum is a solid waste result of the phosphoric acid production, main component of phosphor fertilizers. The phosphogypsum is generated in large scale, causing serious problems of storage. Restriction of environment laws and the increasing cost of the area needed for the phosphogypsum storage have stimulated researches to this material application. Among these researches, there is the reutilization of this waste as construction material of road bases and sub-bases. The samples of theses mixtures were submitted to tests of unconfined compressive strength, indirect tensile strength and California bearing ratio. In the tests of unconfined compressive strength and indirect tensile strength, the specimens were submitted to two test conditions: without immersion and with immersion in water for four hours. It was used 0%, 3%, 5%, 7% e 10% of lime in the mixtures. All specimens were compacted in the energy modified Proctor. Each specimens get through to a process of curing time of the 0, 3, 7 and 28 days. For each condition test 4 copies were molded and the result got by the statistic method of GRUBBS. With this tests, it was concluded that higher values of time of cure and the line content led to higher strength and stiffness values. Besides, test performed after immersion in water presented strength values for the unconfined compressive, diametral compression strength and stiffness lower than those obtained without immersion. It also can be observed that phosphogypsum and lime mixtures got better results of unconfined compressive strength and diametral compression strength than soil and lime mixtures. However, phosphogypsum and cement mixtures got better results of strength and stiffness than phosphogypsum and lime mixtures.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2008-01-31
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.