Thèse de Doctorat
DOI
https://doi.org/10.11606/T.97.2011.tde-27082013-095733
Document
Auteur
Nom complet
Ulysses Padovani
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
Lorena, 2011
Directeur
Jury
Sandim, Hugo Ricardo Zschommler (Président)
Baptista, Carlos Antonio Reis Pereira
Barboza, Miguel Justino Ribeiro
Filgueira, Marcello
Moura Neto, Carlos de
Titre en portugais
Influência dos parâmetros de prensagem isostática a quente na microestrutura e na resistência à fadiga de compósitos WC-Co
Mots-clés en portugais
Carboneto de tungstênio
Fadiga
Prensagem isostática a quente
Resumé en portugais
A presente Tese de Doutorado analisa as modificações induzidas por prensagem isostática a quente (HIP) após a sinterização na resistência à fadiga de compósitos de metal duro com partículas de carboneto de tamanho médio na faixa de 0,6 a 2,0 ?m. A correlação entre a redução de porosidade no processo de prensagem isostática a quente e o aumento de resistência à ruptura transversal é bem conhecida. No entanto, existem questões em relação à eficácia deste processo no aumento da resistência à fadiga, devido à existência de outras imperfeições na microestrutura do material. Um aumento maior na resistência transversal é reportado na literatura para temperaturas de HIP acima do ponto eutético da liga. Os experimentos foram realizados em dois níveis diferentes de pressão de HIP, simulando condições de processo que existem em fornos de média e alta pressão (5,4 MPa e 150 MPa). Também são analisadas duas condições de temperatura de sinterização, 1.350ºC e 1.430ºC. A análise das diferentes condições de processamento mostra que a microestrutura mais homogênea, praticamente sem presença de lagos de cobalto, foi obtida a 1.430°C de temperatura de sinterização e de HIP. Esta condição de processamento resultou em melhores valores de resistência mecânica (estática e dinâmica). As diferenças de microestrutura e propriedades mecânicas obtidas nas duas condições de pressão de HIP (5,4 MPa e 150 MPa) são pouco significativas, tendo maior impacto a correlação entre a microestrutura e propriedades mecânicas em função dos diferentes ciclos de temperatura e tempo de sinterização. A análise das superfícies de fratura do material em fadiga indica uma importante influência de defeitos microestruturais, como regiões alinhadas da fase ? entre grãos de carboneto de tungstênio na iniciação e na propagação da trinca de fratura.
Titre en anglais
Influence of hot isostatic pressing parameters on microstructure and fatigue strength of WC-Co composites
Mots-clés en anglais
Fatigue
Hot isostatic pressing
Tungsten carbide
Resumé en anglais
The present Thesis evaluates modifications induced by hot isostatic pressing (HIP) after sintering on fatigue strength of WC-11Co (in weight %) composites with sintered tungsten carbide grains of 0.6 to 2 ?m. The correlation between decreasing porosity due to hot isostatic pressing process and subsequent increase on transversal rupture strength is well known. Nevertheless, there are questions related to the efficiency of HIP process to increase fatigue strength, mainly due to the existence of microstructure defects besides porosity. An increase on transversal rupture strength is reported in the literature for HIP temperatures above the eutectic point of the composite. Experiments were carried out at two different levels of HIP pressure (5.4 and 150 MPa) covering conditions existing on medium and high pressure furnaces. Two temperatures were also evaluated (1,350 and 1,430°C). The analysis of different processing conditions shows that a more uniform microstructure, without the presence of cobalt lakes, was obtained at a sintering and HIP temperature of 1,430°C. This processing condition also resulted in better statical and dynamical mechanical properties. Microstructure and mechanical properties obtained at two different HIP pressure conditions (5.4 and 150 MPa) were rather similar. Major changes in microstructure and mechanical properties were found as a function of different cycles of temperature and sintering time. Fatigue fracture surfaces were evaluated revealing major influence of microstructural defects such as regions of aligned ? phase where crack initiation and fracture propagation are favored.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
EMT11005.pdf (19.23 Mbytes)
Date de Publication
2013-08-27
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.