• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.97.2012.tde-01102013-105701
Documento
Autor
Nombre completo
Dante Antonucci Dornelas
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
Lorena, 2012
Director
Tribunal
Barboza, Miguel Justino Ribeiro (Presidente)
Coelho, Gilberto Carvalho
Moura Neto, Carlos de
Título en portugués
Caracterização mecânica em temperaturas elevadas da Superliga MAR-M247
Palabras clave en portugués
Alta temperatura
Fluência
MAR-M247
Superligas à base de níquel
Resumen en portugués
A necessidade de trabalhos em altas temperaturas exige o desenvolvimento de materiais com elevada resistência química e mecânica em temperaturas que podem chegar próximas ao seu ponto de fusão. Em especial, os materiais empregados devem apresentar bom comportamento em fluência, de modo a suportar a combinação de altas tensões e altas temperaturas com o mínimo de deformação. O presente trabalho visa caracterizar a superliga MAR-M247, fornecida pela empresa Açotécnica, em condições de fluência para a produção de rotores empregados em turbocompressores automotivos. Os trabalhos são divididos em duas etapas. Na primeira estuda-se a melhor combinação de tratamentos térmicos de solubilização e envelhecimento, chegando à condição de solubilização por 5 horas a 1250?C e envelhecimento por 20 horas a 980?C. Um trabalho de outro aluno (SILVA, 2011) realiza o mesmo estudo para uma variação da superliga MAR-M247 em que o tântalo é totalmente substituído por nióbio. Neste caso, a melhor condição de tratamento é solubilização a 1260?C por 8 h seguida de envelhecimento duplo por 5 h a 880?C e 20 h a 780?C. Na segunda etapa, os materiais dos dois trabalhos, nas melhores condições de tratamento para cada um, são testados em condições de fluência a 850?C a 370, 390, 410 e 430 MPa. A superliga convencional apresenta os maiores valores de vida em fluência enquanto a modificada apresenta os maiores valores de ductilidade. A análise de fratura dos materiais ensaiados a 390 e 430 MPa mostra a presença massiva de carbonetos em toda a extensão da microestrutura, apresentando, em muitos casos, uma morfologia de "escrita chinesa". Apesar disso, todas as amostras apresentam grande quantidade de vazios, indicando que sua nucleação e crescimento são os responsáveis pela fratura do material.
Título en inglés
Mechanical caracterization of MAR-M247 superalloy at high temperatures
Palabras clave en inglés
Creep
High temperature
MAR-M247
Nickel-based superalloys
Resumen en inglés
The needing for high temperature work claim for new materials capable of maintain high strength and good corrosion resistance at temperatures that could reach values near their melting point. Such materials must be creep resistant to withstand high levels of tension and temperature. The aim of this work is the characterization of MAR-M247 under creep conditions for the production of automotive turbocharger rotors made by Açotécnica. The work is split in two steps. In the first one, the material is studied to find the best conditions for solution and ageing heat treatments. The result is a solution treatment at 1250?C for 5 h followed by aging at 980?C for 20 h. A work made by another student (SILVA, 2011) makes the same with a modification of MAR-M247 in which tantalum is completely substituted for niobium. The best condition for this case is a solution treatment at 1260?C for 8 h and a double aging treatment at 880?C for 5 h and 780?C for 20 h. At the second part of the work, both the materials are tested under creep conditions at 850?C with 370, 390, 410 and 430 MPa. The conventional superalloy shows the highest values for creep strength and the modified superalloy shows the highest ductility. Fracture surfaces for 390 and 430 MPa showed brittle carbides with "chinese script" morphology. Conversely, holes are present on all four materials what shall mean that its nucleation and growth was the most probably fracture path.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
EMD12002_C.pdf (3.91 Mbytes)
Fecha de Publicación
2013-10-01
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.