Master's Dissertation
DOI
https://doi.org/10.11606/D.85.2019.tde-18112019-111622
Document
Author
Full name
Elton Danilo Cavalheira
E-mail
Institute/School/College
Knowledge Area
Date of Defense
Published
São Paulo, 2019
Supervisor
Committee
Takiishi, Hidetoshi (President)
Bock, Eduardo Guy Perpétuo
Silva, Suelanny Carvalho da
Title in Portuguese
Caracterização mecânica e microestrutural do zircaloy-4 obtido por HD e metalurgia do pó
Keywords in Portuguese
metalurgia do pó
reciclagem
usinagem
zircaloy-4
Abstract in Portuguese
A etapa de usinagem para fabricação de tubos e tampões (end caps) de Zircaloy-4 (Zr-4) utilizados em reatores nucleares à água pressurizada (reatores PWRs) geram grandes quantidades de rejeitos deste material. Devido ao alto custo do Zr-4 faz-se necessário sua reciclagem, que representa uma grande economia para a política Nuclear Brasileira e também evita seu descarte para o meio ambiente. Neste trabalho, os rejeitos da usinagem do Zr-4 foram aquecidos em atmosfera de hidrogênio (923 K), sendo o pó resultante desta etapa, peneirado em malha 200 e 325 mesh (<75 e <45 μm). Nesta etapa, foram retirados os materiais que não absorvem hidrogênio proveniente da usinagem, diminuindo a contaminação final por Fe da liga Zr-4. A moagem foi realizada em moinho de alta energia, utilizando pote e esferas de zircônia para diminuir a contaminação do pó. Os experimentos foram realizados em diferentes tempos de moagem (0 a 120 min). A amostra foi prensada a 200 MPa (prensagem isostática) e sinterizada a 1423 K por 10 h. A microestrutura foi analisada por microscopia eletrônica de varredura (MEV) e foi determinada a microdureza Vickers. Os resultados mostraram que após 60 min de moagem o tamanho médio das partículas foi de 2,4 μm. a microdureza Vickers após sinterização foi de 425 HV e tamanho médio de grão em torno de 50 μm. As amostras apresentaram valores de densidade hidrostática de 99% em relação à teórica, e a microestrutura apresentou morfologia típica do Zr-4 da fase α e grãos equiaxiais. Para redução de áreas de armazenamento dos cavacos obteve-se uma redução de 27 vezes no volume ocupado após hidretação, cominuição e prensagem. Foi possível usinar os tampões a partir das amostras com menor medida de microdureza.
Title in English
Mechanical and microstructural characterization of zircaloy-4 obtained by HD and powder metallurgy
Keywords in English
machining
powder metallurgy
recycling
zircaloy-4
Abstract in English
The machining step for manufacturing Zircaloy-4 (Zr-4) tubes and end caps used in pressurized water nuclear reactors (PWRs) to generate large amounts of tailings from this material. Due the high cost of the Zr-4 its requires recycling, which represents a great economy for Brazilian Nuclear policy and also avoids its disposal to the environment. In this work, the machining chips of Zr-4 were heated in the hydrogen atmosphere (923 K), and the powder from this step was sieved in the 200 and 325 mesh (<75 and <45 μm). In this stage, materials that did not absorb the hydrogen proven by the machining were removed, reducing the final contamination by Fe of the Zr-4 alloy . Grinding was performed in the high energy mill, using zirconia pot and spheres to reduce contamination. The experiments were performed at different milling times (0 to 120 min). One sample was pressed at 200 MPa (isostatic pressure) and sintered at 1423 K for 10 h. The microstructure was analyzed by scanning electron microscopy (SEM) and Vickers microhardness was determined. . The results showed that after 60 min milling the average particle size was 2.4 μm, Vickers microhardness after sintering was 425 HV and average grain size around 50 μm. The samples shown hydrostatic density values of 99% compared to the theoretical, and a microstructure shows typical morphology of phase alpha of Zr-4 and equiaxial grains. To reduce chip storage areas, a reduction of 27 times in the volume occupied by the chips after hydration, comminution and pressing was obtained. It was possible to machine the end caps from the samples with the lowest microhardness measurement.
 
WARNING - Viewing this document is conditioned on your acceptance of the following terms of use:
This document is only for private use for research and teaching activities. Reproduction for commercial use is forbidden. This rights cover the whole data about this document as well as its contents. Any uses or copies of this document in whole or in part must include the author's name.
Publishing Date
2019-12-03
 
WARNING: Learn what derived works are clicking here.
All rights of the thesis/dissertation are from the authors
CeTI-SC/STI
Digital Library of Theses and Dissertations of USP. Copyright © 2001-2024. All rights reserved.