Mémoire de Maîtrise
DOI
https://doi.org/10.11606/D.85.2019.tde-13062019-152512
Document
Auteur
Nom complet
Amon Solano Lopes Ribeiro
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Paulo, 2019
Directeur
Jury
Lazar, Dolores Ribeiro Ricci (Président)
Marchi, Juliana
Saavedra, Guilherme de Siqueira Ferreira Anzaloni
Titre en portugais
Efeitos da sinterização por micro-ondas nas propriedades microestruturais e mecânicas de cerâmicas 3Y-TZP
Mots-clés en portugais
microestrutura
propriedades mecânicas
sinterização por micro-ondas
Y-TZP
Resumé en portugais
As técnicas de sinterização convencional de zircônia tetragonal parcialmente estabilizada com ítria (Y-TZP) vêm apresentando limitações quanto ao tempo e temperatura de sinterização, aumentando o custo do produto biocerâmico. Assim, a sinterização por micro-ondas se torna uma alternativa apropriada promovendo rápido aquecimento, elevadas densidades, controle de tamanho de grão, reduzindo o tempo total para produzir o material cerâmico desejado. O objetivo do presente trabalho foi comparar o efeito da sinterização por micro-ondas de cerâmicas comerciais Y-TZP pré-sinterizadas (grupos V-M e LP-M) e outra produzida a partir de pós sintetizados pela técnica de coprecipitação (grupo CP-M). Valores de densidade, tenacidade à fratura, tamanho de grão, translucidez e quantificação das fases cristalinas de amostras sinterizadas, antes e após envelhecimento em reator hidrotérmico, foram relatados. Os grupos V-M e CP-M de amostras foram sinterizados a 1450°C e 1350°C por 15 e 30 minutos e o grupo LP-M, sinterizado apenas a 1450°C, nos mesmos tempos. Os grupos sinterizados a 1450°C por 15 e 30 minutos apresentaram os maiores valores de densidade (média de 98% em relação à densidade teórica). O tamanho médio de grão das amostras de maior densificação variou de 309 a 355 nm. Os resultados de translucidez (ΔE) são próximos aos divulgados na literatura. A quantificação de fases por difratometria de raios X das amostras não envelhecidas, indicou que em sua maioria, são formadas por 89% de fase tetragonal e 11% fase cúbica. Os ensaios de envelhecimento hidrotérmico permitiram verificar o comportamento de degradação de fases das amostras sinterizadas em micro-ondas, demonstrando que, no caso das cerâmicas comerciais, essa técnica é uma alternativa viável para produção de cerâmicas Y-TZP mais resistentes à degradação.
Titre en anglais
Microwave sintering effects on 3Y-TZP microstructural and mechanical properties
Mots-clés en anglais
mechanical properties
microstructure
microwave sintering
Y-TZP
Resumé en anglais
Conventional sintering techniques of yttria-tetragonal zirconia polycrystals (Y-TZP) ceramics have presented limitations regarding the sintering time and temperature, increasing the cost of the final dental and biomedical products. Herein, microwave sintering comes to be an interesting alternative by providing fast heating, high densification and grain size control, reducing the overall processing time to produce the desired ceramic material. The aim of this study was to compare the effect of microwave sintering of a pre-sintered Y-TZP dental ceramics (V-M and LP-M groups) and other prepared from powders synthesized in a laboratorial scale by the precipitation route (CP-M group). Values of densification, fracture toughness, grain size, translucency and crystalline phases quantification of aged and non-aged sintered samples were reported. The groups V-M and CP-M were sintered at 1450°C and 1350°C for 15 and 30 minutes and the group LP-M was sintered at 1450°C at the same times. The sintered samples at 1450°C for 15 and 30 minutes presented the highest density values (around 98% related to theoretical density). The average grain size of highest density samples varied between 309 a 355 nm. The translucency (ΔE) results were similar to the reported literature. The X-ray diffraction crystalline phase quantification analysis indicated that the majority of the non-aged samples were formed by 89% tetragonal phase and 11% cubic phase. The hydrothermal tests allowed to verify the phase degradation behavior under wet environment of microwave sintered samples, indicating that in the case of commercial ceramics, this technique as an viable alternative for production of better degradation resistance Y-TZP ceramics.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2019-06-28
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.