• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.85.2016.tde-05092016-085643
Documento
Autor
Nombre completo
Antonio Paulo Rodrigues Fernandez
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Paulo, 2016
Director
Tribunal
Faria Júnior, Rubens Nunes de (Presidente)
Ett, Gerhard
Wendhausen, Paulo Antônio Pereira
Título en portugués
Estudo das características elétricas e microestruturais de supercapacitores para armazenamento de energia
Palabras clave en portugués
capacitância
capacitor de dupla camada elétrica
resistência em paralelo equivalente
resistência em série equivalente
supercapacitores
Resumen en portugués
Esta dissertação tem por objetivo reportar dados relativos às características elétricas e microestruturais de eletrodos aplicadas em dispositivos armazenadores de energia, especificamente supercapacitores constituídos por eletrodos de carvão ativado. Os parâmetros elétricos estudados foram a resistência em série equivalente obtida pelo método da interrupção de corrente (ESR(Inst)) (sendo que a sigla ESR é oriunda do termo inglês Equivalent Series Resistance), a resistência em paralelo equivalente (EPR(Dep)) obtida pelo método do valor dependente (sendo que a sigla EPR é oriunda do termo inglês Equivalent Parallel Resistance) e a capacitância (C(DC)) obtida pelo método da corrente contínua (sendo que a sigla DC oriunda do termo inglês Direct Current). Tais parâmetros foram escolhidos devido ao impacto que causam no tempo de vida útil, na capacidade de armazenamento de cargas elétricas, na velocidade de carga e descarga, na perda por efeito termoiônico nos processos de carga e descarga e na perda de cargas armazenadas devido à autodescarga em supercapacitores. Os dados microestruturais reportam por meio de imagens a homogeneidade da porosidade e por meio de valores correlacionados a composição química e eventuais contaminações presentes nos eletrodos. Os dados e valores coletados possuem a intenção de servir como referência comparativa de qualidade e apontar qual parâmetro afeta mais a qualidade do supercapacitor. Para tanto foram realizados testes a fim de coletar valores de C(DC), ESR(Inst) e EPR(Dep) após a exposição de supercapacitores de 1F/5,5V a temperaturas de 50ºC, 75ºC, 100ºC e 125ºC por 672 horas, sendo os dados coletados ao inicio dos testes, à temperatura ambiente, e posteriormente a cada 168 horas. Feitos os experimentos concluiu-se que o parâmetro que sofreu maior deterioração com o acréscimo de energia térmica foi a EPR(Dep), em seguida a C(DC), que de fato pouco sofreu alteração e a ESR(Inst), em que a mudança dentro do erro de medição foi imperceptível.
Título en inglés
Study of electrical and microstructural characteristics of supercapacitors for energy storage
Palabras clave en inglés
capacitance
EDLC
equivalent parallel resistance
equivalent series resistance
supercapacitors
Resumen en inglés
This paper aims to report information on electrical and microstructural characteristics of electrodes applied at devices that store energy, specifically supercapacitors made of activated carbon electrodes. The studied electrical parameters were the equivalent series resistance obtained by the method of the instantaneous value of the voltage drop (ESR(Inst)), where the acronym ESR has the meaning Equivalent Series Resistance, the equivalent parallel resistance (EPR(Dep)) obtained by the method of dependent value, where the acronym EPR has the meaning Equivalent Parallel Resistance, and the capacitance (C(DC)) obtained by the method of direct current. These parameters were chosen because of the impact they have on lifetime, the storage capacity of electric charge, the speed of loading and unloading, the loss thermionic effect on the charge and discharge processes and loss of stored charge due to self-discharge in supercapacitors. The data given by microstructural images of the homogeneity and porosity values correlated by the chemical composition and possible contaminations present in the electrodes. The collected data and values are intended to serve as a comparative reference point and quality parameter which most affects the quality of the supercapacitor. For both tests were carried out in order to collect values of C(DC), ESR(Inst) and EPR(Dep) after supercapacitors of the 1F/5.5V are exposure at temperatures of 50, 75, 100 and 125°C for 672 hours, and the data collected at the beginning of the tests (room temperature) and subsequently every 168 hours. Made experiments it was concluded that the parameter further deterioration suffered with the increase of thermal energy is EPR(Dep), then C(DC), which in fact little changed and ESR(Inst), in which the change in the measurement error was are noticeable.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2016-09-16
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.