• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.85.2009.tde-01092009-153704
Documento
Autor
Nombre completo
Horacio Marconi da Silva Matias Dantas Linhares
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Paulo, 2009
Director
Tribunal
Ranieri, Izilda Marcia (Presidente)
Gomes, Laércio
Hernandes, Antonio Carlos
Título en portugués
Síntese e caracterização de cristais de KY3F10 e KY3F10:Yb:Nd:Tm para aplicações ópticas
Palabras clave en portugués
crescimento de cristais
espectroscopia de lantanídeos
KY3F10
terras raras
Resumen en portugués
Neste trabalho foram crescidos cristais de KY3F10 puros e dopados com Yb, Nd e Tm, visando à obtenção de emissão no azul através de conversão ascendente dos íons de Tm3+. Foram estabelecidas as melhores condições para a síntese e purificação de cristais de KY3F10. Os cristais dopados com 1,3 mol% de Nd, 0,5 mol% de Tm e concentrações variáveis de Yb (5, 10, 20, 30 e 40 mol%) foram obtidos através do resfriamento lento dos lingotes a partir da fusão, utilizando-se um sistema de síntese convencional e em uma atmosfera reativa de HF. Os parâmetros estudados para a obtenção destes cristais foram as taxas de resfriamento e diferentes configurações de barquinhas. Foi também determinado um limite de concentração de itérbio de 30mol% para a formação de única fase cúbica, para as taxas de resfriamento utilizadas neste trabalho. A caracterização química e física das amostras foi efetuada por difração de raios-X, análise térmica diferencial, espectrometria de emissão óptica por plasma acoplado indutivamente (ICP-OES), microscopia eletrônica de varredura, absorção e emissão ópticas. Um estudo espectroscópico inicial foi realizado para verificar o efeito da concentração de itérbio na eficiência de emissão no azul para o cristal de KY3F10:Yb:Nd:Tm. Quando o íon de Nd é bombeado em 797nm, determinou-se que as concentrações apropriadas de Yb devem estar entre 10 e 20 mol% para a emissão em 480nm e entre 20 e 30 mol% para a emissão em 450nm. Observou-se também que as emissões no ultravioleta (350 e 360nm) cresceram consideravelmente com o aumento de Yb3+ na amostra.
Título en inglés
SYNTHESIS AND CHARACTERIZATION OF KY3F10 AND KY3F10:Yb:Nd:Tm CRYSTALS FOR OPTICAL APPLICATIONS
Palabras clave en inglés
crescimento de cristais
espectroscopia de lantanídeos
KY3F10
terra raras
Resumen en inglés
In this work, crystals of KY3F10 pure and doped with Yb, Nd and Tm were grown aiming at the attainment of blue emission via Tm3+ ions upconversion. It was established the best conditions to synthesis and purification of KY3F10. Crystals doped with 1.3 mol% Nd, 0.5 mol% Tm and some concentrations of Yb (5, 10, 20, 30 and 40 mol%) were obtained by slow cooling of the charge from the melt, using an usual conventional synthesis system and in a reactive HF atmosphere. It was taken into account parameters as cooling rate and different configurations of boats to conditioning the materials. The limit of Yb concentration to obtain a unique cubic phase was determined as 30mol%, for the cooling rates used in this work. The physical and chemical characterizations of the samples were performed by X-ray diffraction, differential thermal analysis, inductively coupled plasma-optical emission spectroscopy (ICP-OES), scanning electron microscopy, optical absorption and emission. An initial spectroscopic study was performed to verify the effect of the Yb3+ concentration regarding the blue emission efficiency in the KY3F10:Yb:Nd:Tm. When the Nd3+ is pumped at 797 nm, it was determined that the suitable Yb concentrations are between 10 and 20 mol% to obtain blue emission at 480 nm, and between 20 and 30 mol% to obtain emission at 450 nm. It was observed that two emissions bands in the UV (350 and 360nm) enhanced proportionally with the Yb3+ concentration.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2009-09-23
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.