Thèse de Doctorat
DOI
https://doi.org/10.11606/T.85.2015.tde-21122015-150412
Document
Auteur
Nom complet
João Francisco Trencher Martins
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Paulo, 2015
Directeur
Jury
Hamada, Margarida Mizue (Président)
Chubaci, Jose Fernando Diniz
Pereira, Maria da Conceição Costa
Santos, Adir Janete Godoy dos
Watanabe, Shigueo
Titre en portugais
Influência de defeitos e da qualidade superficial no desempenho do cristal de iodeto de mercúrio aplicado como detector de radiação
Mots-clés en portugais
detector
HgI2
iodeto de mercúrio
semicondutor
temperatura ambiente
Resumé en portugais
Os compostos semicondutores com alto número atômico e energia de banda proibida larga vêm sendo pesquisados como detectores de radiação X e gama, com alta resolução energética, operando à temperatura ambiente. O denominador comum dos materiais semicondutores, que operam à temperatura ambiente, é a dificuldade em crescer cristais com pureza química elevada e boa estequiometria. O desenvolvimento deste tipo de detectores semicondutores de radiação é ainda um desafio tecnológico e tem deparado com muitos fatores limitantes, tais como: material de partida com qualidade compatível para o uso no crescimento de cristal, baixa estabilidade do detector ao longo do tempo, oxidação superficial e outras dificuldades relatadas na literatura, que limitam o seu uso. Neste trabalho, estabeleceu-se a metodologia de transporte físico de vapor (PVT) para a purificação e crescimento do cristal semicondutor de Iodeto de Mercúrio (HgI2). Cristais de HgI2 com orientação cristalina, estequiometria e morfologia da superfície adequadas foram obtidos por essa técnica. Uma redução nítida de impurezas após a purificação pode ser observada e o nível de impureza presente nos cristais não interferiu nas suas estruturas cristalinas. Uma boa morfologia com uniformidade nas camadas da superfície foi encontrada nos cristais, indicando uma boa orientação na estrutura cristalina. Um estudo inédito foi realizado no Laboratório da University of Freiburg, sob a coordenação do Prof. Michael Fiederle, com o intuito de aumentar a estabilidade do detector de HgI2 ao longo do tempo. A aplicação de diferentes tipos de resina polimérica para encapsulamento dos detectores HgI2 foi realizada e estudada, no intuito de proteger o cristal de HgI2 das reações com os gases atmosféricos e isolar eletricamente a superfície dos cristais. Quatro resinas poliméricas foram analisadas, cujas composições são: Resina n 1: 50% - 100% de heptano, 10% - 25% metilcicloexano, <1% de ciclo-hexano; Resina n2: 25% - 50% de etanol, 25% - 50% de acetona, <2,5% de acetato de etilo; Resina n3: 50% - 100% de acetato de metilo, 5% - 10% de n-butilo e Resina 4: 50% - 100% de etil-2- cianoacrilato. A influência dos tipos de resina polimérica utilizada na espectroscopia de desempenho do detector semicondutor HgI2 é, claramente, demonstrada. O melhor resultado foi encontrado para o detector encapsulado com resina n3. Um aumento de até 26 vezes no tempo de estabilidade, como detector de radiação, foi observado para os detectores encapsulados com resina em comparação com o detector não encapsulado, exposto à atmosfera.
Titre en anglais
The influence of defects and surface quality on the mercuric iodide crystal used as a radiation detector
Mots-clés en anglais
detector
HgI2
mercuric iodide
room temperature
semiconductor
Resumé en anglais
The semiconductor compounds with high atomic number and wide band gap energy have been investigated as X and gamma range radiation detectors, with high energy resolution, operating at room temperature. The common denominator of semiconductor materials, which operate at room temperature, is the difficulty to grow crystals with high chemical purity and good stoichiometry. The development of this type of radiation semiconductor detectors is still a technological challenge and it has faced many limiting factors, such as: starting material quality compatible for use in crystal growth, low stability of the detector over the time, surface oxidation and other difficulties reported in the literature, which limit their use. In this work, the Physical vapor transport (PVT) methodology for purification and growth of the Iodide Mercury (HgI2) semiconductor crystals was established. HgI2 crystals with crystalline orientation and suitable surface stoichiometry and morphology were obtained by this technique. A significant reduction of impurities after purification could be observed and the impurity levels present in crystals did not interfere in their crystal structures. A good morphology with uniformity in the surface layers of the crystals was found, indicating a good orientation in the crystal structure. A novel study was conducted at the Laboratory of the University of Freiburg, under the guidance of Prof. Michael Fiederle, in order to increase the stability of the HgI2 detector over the time. The application of different types of polymer resins for encapsulation of HgI2 detectors was carried out and studied, in order to protect the HgI2 crystal of reactions with the atmospheric gases and to isolate, electrically, the surface of these crystals. Four types of polymeric resins were evaluated, and each composition is : (a) Resin n1: 50% - 100% heptane 10% - 25% methyl cyclohexane, <1% cyclohexane; (b) Resin n2: 25% - 50% ethanol, 25% - 50% acetone <2.5% ethyl acetate; (c) Resin n3: 50% - 100% methyl acetate, 5% - 10% n-butyl and (d) Resin n 4: 50% - 100% ethyl-2- cyanoacrylate. The influence of the different types of polymer resins composition, used in the HgI2 detector encapsulation, is clearly demonstrated by the results of the gamma ray spectroscopy. The best results were found for the detector encapsulated with resin n3. An increase of up to 26 times in the stability period was observed for the detectors encapsulated with resin, compared to those which were not encapsulated and, therefore, had been exposed to the atmosphere.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2015-12-28
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.