• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.54.1983.tde-24062008-160115
Documento
Autor
Nombre completo
Dayse Iara dos Santos
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Carlos, 1983
Director
Tribunal
Aegerter, Michel Andre (Presidente)
Craievich, Aldo Felix
Zanotto, Edgar Dutra
Título en portugués
Vidros porosos de de alto teor de sílica para armazenamento de rejeitos nucleares. Solidificação, caracterização e lixiviação
Palabras clave en portugués
Armazenamento de rejeitos nucleares
Lixivação
Separação de fases
Testes soxlet
Vidro poroso de sílica
Resumen en portugués
Apresentamos um estudo de solidificaçaõ e lixiviacão de matrizes de vidros porosos de alto teor de sílica armazenando 20% em peso de solução aquosa simuladora de rejeitos nucleares de alto nível de radioatividade do tipo Savanah River Labratory. A matriz porosa foi preparada após o tratamento térmico de um vidro de 65% SiO2-27%B2O3-8%Na2O, que sofreu separação de fase à 560°C por 20 horas e lixiviado em HCl - 3N à 90°C. O tamanho dos poros (tipicamente de 100 à 250Å de diâmetro) , foi determinado utilizando o método BET. Após sinterização à 1300°C em ar, as amostras foram caracterizadas física e quimicamente através de testes de lixiviação padronizados MCC1, Soxhlet (MCC5) e Estagnante durante cerca de 28 dias. Determinamos a perda de peso total, o pH, as taxas de lixiviação diferencial e as concentrações acumuladas para os seguintes elementos: Si, Na, B, Ca, Mn, Al, Fe e Ni com técnicas de ICP e espectroscopia de chama para o caso do Na. Os resultados são comparados com os obtidos com vidros borosilicatos de referência, fabricados por fusão convencional (SRL 131, PNL 76-68, MCC 76-68, SRL TDS 131, AVM-Ml à M7), vidros fabricados pela técnica sol-gel (TDS 211), vidros de alto teor de sílica (CU PGM), synroc-D, cerâmicas manufaturadas, concreto FUETAP e matrizes metálicas. Os valores obtidos são similares àqueles obtidos com os melhores vidros borosilicato presentemente usados.
Título en inglés
High content silica porous glass for nuclear waste storage. Solidification, characterization and leaching
Palabras clave en inglés
Corrosion of waste storage
Leaching
Nuclear waste storage
Phase separation
Silica porous glass
Soxlet tests
Resumen en inglés
We present a study of the sinterization and of the leaching behavior of a high silica porous glass matrix containing 20 weight % of simulated solution of high level liquid nuclear waste of the type Savanah River Laboratory. The porous matrix has been prepared after heat treatment of a 65% SiO2-27%B2O3-8%Na2O glass, phase separate at 560°C for 20 hours and leached in 3N HCl at 90°C. The pore size (typically 100-250Å in diameter) has been determined by the BET method. After sinterization in air at 1300°C, the samples have been physically and chemically characterized during 28 days using the MCC1, Estagnant and Soxhlet (MCC5) standard tests. We have determined thetotal weight loss, the pH, the diferential leaching rate and the cumulative concentrations for the following elements: Si, Na, B, Ca, Mn, Al, Fe and Ni by ICP technique, for Na flames spectroscopy. The results are compared with these obtained with other reference borosilicate glasses made by conventional fusion techniques (SRL 131, PNL 76-68, MCC 76-68, SRL TDS 131, AVM-M1 to M7), glasses made by sol-gel technique (TDS-211), porous glasses matrix (CU PGM), synroc-D, tailored ceramics, FUETAP concrete and metallic matrix. The values obtained are similar to those found for the best borosilicate glass presently used.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
DayseSantos_M.pdf (4.03 Mbytes)
Fecha de Publicación
2008-07-04
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.