Mémoire de Maîtrise
DOI
https://doi.org/10.11606/D.54.1992.tde-07112013-173606
Document
Auteur
Nom complet
Nilton Guedes da Silva
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Carlos, 1992
Directeur
Jury
Oliveira Junior, Osvaldo Novais de (Président)
Canevarolo Junior, Sebastião Vicente
Gregório Filho, Rinaldo
Titre en portugais
Preparação e caracterização dos copolimeros P (VDF-TrFE).
Mots-clés en portugais
Copolímeros
Ferroeletricidade
Filmes finos
Resumé en portugais
Esta dissertação descreve os métodos empregados na preparação por solução de filmes de copolímeros P(VDF-TrFE) nas composições molares 60/40, 70/30 e 80/20. Foram utilizadas as técnicas de deposição por centrifugação (spin coating deposition) e de espalhamento por extensor, usando acetona e metil-etil-cetona (MEK) como solventes. Filmes de boa qualidade só foram obtidos quando se acelerou o processo de evaporação do solvente, através da passagem de um fluxo de ar seco na câmara onde os filmes eram produzidos. Medidas de espectroscopia de infra-vermelho confirmaram a ausência de solvente nos filmes, já que observou-se que o pico 1715 cm-1 (carbonilha) característico do MEK não aparece nos resultados com filmes. A caracterização dos filmes fabricados foi feita através de medidas de calorimetria diferencial exploratória de varredura (DSC), difração de raios-X, espectroscopia de infra-vermelho e cromatografia líquida por exclusão de tamanho (GPC). Nos termogramas de DSC puderam ser identificadas as transições de fase ferro-paraelétrica (na temperatura de Curie, Tc) e de fusão. Os valores de Tc e da temperatura de fusão, Tf, encontrados são consistentes com os valores da literatura, com Tc aumentando com o conteúdo de VDF, ao passo que o oposto ocorre com Tf, devido ao fato que o aumento do percentual de TrFE na região cristalina aumenta a estabilidade da fase paraelétrica. Os difratogramas de Raios-X apresentaram, basicamente, um ombro largo correspondente à porção amorfa do filme, e um pico alto e estreito devido a parte cristalina do filme. No ajuste dos difratogramas através de uma função de Lorentz modificada, os resultados para as amostras de 60/40 e 70/30 foram ajustadas com três picos, o que parece indicar que pode haver duas fases cristalinas para estas amostras. Já os resultados para a amostra de 80/20 foram ajustados com apenas dois picos. O tratamento térmico das amostras, a diversas temperaturas, mostrou influenciar fortemente as propriedades dos filmes. Os seus efeitos mais importantes são o aumento da temperatura de Curie e da percentagem de cristalinidade do filme com a temperatura de tratamento
Titre en anglais
Preparation and characterization of P(VDF-TrFE) copolymers
Mots-clés en anglais
Copolymers
Ferroelectricity
Thin films
Resumé en anglais
This dissertation describes the experimental methods employed in the fabrication of thin films (up to 40 micra) of the copolymer P(VDF-TrFE) for three different VDF contents, Viz. 60/40, 70/30 and 80/20. The copolymers were dissolved in either acetone or methyl-ethyl-ketone(MEK) and deposited on a solid substrate using spin coating or a sliding-knife. Good quality films could only BR obtained after dry air was flushed into the chamber where the films were fabricated. Infra-red spectrocopy measurements confirmed the abscene of solvent in the samples, as the 1715 cm-1 peak from MEK is not present in the results for the films. The film characterization was carried out using differential scanning calorimetry (DSC), X-ray diffraction, infra-red spectrocopy and gel permeation chromatography (GPC). Phase transitions could be identified in the DSC thermography which can be related to the ferro-paraelectric transition (at the Curie temperature, Tc) and to the melting of the sample. The values for Tc and the melting temperature, Tf), were consistent with those published in the literature, with Tc increasing with the contents of VDF, while the opposite is true for Tf because the increase in the TrFE contents causes the stability of the paraelectric phase to increase. The X-ray diffractograms displayed, basically, one broad halo due to the amorphous part of the film, and a eak due to its crystalline region. The diffractograms were fitted using a modified Lorentz function, where three peaks had to be assumed for the 60/40 and 70/30 samples. This appears to indicate that there may exist two crystalline phases in these samples. The results for 80/20 samples, on the other hand, were fitted with two peaks. The thermal treatment of the samples, under various temperatures, proved to influence strongly the properties of the films. Its main effects are the increase in the Curie temperature and the increase in the degree of crystallinity of the films with increasing temperature of thermal treatment
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2013-11-08
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.