Master's Dissertation
DOI
https://doi.org/10.11606/D.43.2018.tde-03052018-111901
Document
Author
Full name
Bianca Jardim Mendonça
E-mail
Institute/School/College
Knowledge Area
Date of Defense
Published
São Paulo, 2018
Supervisor
Committee
Chubaci, Jose Fernando Diniz (President)
Silva, Antonio Ferreira da
Tatumi, Sonia Hatsue
Title in Portuguese
Produção e caracterização de filmes finos de TiO2
Keywords in Portuguese
anatase
band gap
constante dielétrica
dióxido de titânio
magnetron sputtering
rutila
Abstract in Portuguese
Nesse trabalho foram fabricados filmes finos de TiO2 por RF magnetron sputtering reativo sobre substrato de silício (1 0 0). A pressão parcial do oxigênio na câmara foi variada de 5 a 100% em relação ao argônio. Após a deposição os filmes foram submetidos a tratamento térmico em atmosfera de oxigênio. A estequiometria dos filmes e o perfil de profundidade foram obtidos por RBS. A estrutura cristalina foi obtida por XRD. As propriedades ópticas foram obtidas por interferometria e reflectância e as elétricas por meio das curvas C-V. Os valores de espessura dos filmes sem tratamento térmico aumentaram aproximadamente 41% com o aumento do oxigênio na câmara de deposição. Essa variação está ligada ao aumento da eficiência do sputtering do alvo. Os índices de refração dos filmes sem tratamento térmico se mantiveram dentro de um intervalo de aproximadamente 2,3 a 2,4. A diminuição do band gap com o tratamento térmico é consequência da mudança de fase cristalográfica de anatase para rutila. A estequiometria TiOx dos filmes antes do tratamento térmico apresentaram valores de x entre 2,0 e 2,4. A espessura em TFU dos filmes aumentou com o percentual de oxigênio na câmara. As amostras que receberam tratamento térmico apresentaram difusão de titânio na interface do substrato e incorporação de oxigênio no filme. Os valores da constante dielétrica aumentaram com o percentual de oxigênio na câmara, em contraposição com o efeito do tratamento térmico que diminuiu o valor. Todos os resultados observados são coerentes do ponto de vista da mudança de fase anatase rutila e aumento do percentual de oxigênio na câmara.
Title in English
Production and Characterization of TiO2 Thin Films
Keywords in English
anatase
band gap
dielectric constant
magnetron sputtering
rutile
titanium dioxide
Abstract in English
In this work thin films of TiO2 were produced by reactive RF magnetron sputtering on silicon substrate (1 0 0). The oxygen partial pressure in the chamber was varied from 5 to 100% in relation to argon. After deposition the films were submitted to thermal treatment under an oxygen atmosphere. The stoichiometry of the films and the depth profile were obtained by RBS. The crystal structure was obtained by XRD. Its optical properties were obtained by interferometry and reflectance and the electrical were obtained by means of the C-V curves. The thickness values of films without heat treatment increased approximately 41% with the increase of oxygen in the deposition chamber. This variation is linked to the increased sputtering efficiency of the target. The refractive indexes of films without heat treatment remained within a range of about 2.3 to 2.4. The decrease of the band gap with the heat treatment is a consequence of the change of crystallographic phase from anatase to rutile. The TiOx stoichiometry of the films before the heat treatment showed values of x between 2.0 and 2.4. The TFU thickness of the films increased with the percentage of oxygen in the chamber. The samples that received heat treatment shows diffusion of titanium at the interface of the substrate and incorporation of oxygen in the film. The values of the dielectric constant increased with the percentage of oxygen in the chamber, as opposed to the effect of the thermal treatment that decreased the value. All the results observed are consistent from the point of view of the anatase - rutile phase transition and the increase in the oxygen percentage in the chamber.
 
WARNING - Viewing this document is conditioned on your acceptance of the following terms of use:
This document is only for private use for research and teaching activities. Reproduction for commercial use is forbidden. This rights cover the whole data about this document as well as its contents. Any uses or copies of this document in whole or in part must include the author's name.
Publishing Date
2018-05-04
 
WARNING: Learn what derived works are clicking here.
All rights of the thesis/dissertation are from the authors
CeTI-SC/STI
Digital Library of Theses and Dissertations of USP. Copyright © 2001-2024. All rights reserved.