Mémoire de Maîtrise
DOI
https://doi.org/10.11606/D.3.2019.tde-30012019-141410
Document
Auteur
Nom complet
Pedro Forastieri de Almeida Prado
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Paulo, 2018
Directeur
Jury
Espinosa, Denise Crocce Romano (Président)
Moraes, Viviane Tavares de
Zilles, Roberto
Titre en portugais
Reciclagem de painéis fotovoltaicos e recuperação de metais.
Mots-clés en portugais
Hidrometalurgia
Metais (Recuperação)
Paineis (Reciclagem)
Resumé en portugais
Com a expansão do emprego de módulos fotovoltaicos para geração energética, surge o desafio do descarte adequado desse resíduo de equipamento eletroeletrônico. Através da elaboração de um processo multietapas, esse desafio torna-se possível de ser abordado. O presente estudo possui o objetivo de recuperar os materiais presentes nos módulos fotovoltaicos de silício cristalino e de silício amorfo. Diversas técnicas de caracterização física e química foram empregadas para determinar-se composição dos módulos fotovoltaicos e consequentemente o fluxo de processos necessários para recuperação dos materiais identificados. Foi identificado que o módulo de silício cristalino possuía no semicondutor alguns metais como prata (na concentração de 0,063% em massa do módulo) e silício, e na fase polimérica polidimetilsiloxano como encapsulante e PET como backsheet. A separação e recuperação dos polímeros foi realizada através do uso da teoria de dissolução de solventes de Hildebrand, abordando aspectos termodinâmicos e cinéticos. A separação ocorreu em 24h a 860rpm mergulhando-se os módulos em isopropanol, podendo ocorrer separação em até 6h a 860rpm utilizando-se tetrahidrofurano. A lixiviação da prata a partir do semicondutor foi possível com ácido sulfúrico 4mol.L-1, 95°C, sob adição de 6mL de peróxido de hidrogênio a cada 15min, alcançando-se 100% de lixiviação em 2h. Alterando-se a temperatura para 30°C a lixiviação foi completa apenas em 6h de experimento Precipitou-se a prata em solução na forma de cloreto de prata com adição de cloreto de sódio. O módulo de silício amorfo continha EVA na fração polimérica e silício, germânio, prata, estanho e índio (concentração 0,34g/m2 do módulo) na fração metálica, observados tanto por micrografias quanto por análise química quantitativa. A calcinação a 400°C permitiu a remoção do EVA e liberação dos contatos de prata. A lixiviação de índio foi de 100% para uma solução 1mol.L-1 de ácido fosfórico a 75°C, sob 800rpm de agitação e relação sólido-líquido 1g.10mL-1 em 1h.
Titre en anglais
Recycling of photovoltaic modules and metals recovery.
Mots-clés en anglais
Hydrometallurgy
Photovoltaic modules
Polymeric dissolution
Recycling
Resumé en anglais
As the photovoltaic module market grows, an increasingly challenging scenario arises for solar modules end of life management. Such a scenario can be tackled through a process comprising multiple steps. This study has the objective to recover materials present in photovoltaic modules of crystalline silicon and amorphous silicon. Several characterization techniques (physical and chemical) were employed to determine the composition of the modules and thus the process flow needed to recover the identified materials. Along the process, it was noticed that the crystalline silicon module had in its semiconductor metals such as silver (in concentration of at least 0,063% in weight of module) and silicon. Also polydimethylsiloxane was identified as encapsulant and polyethylene therephtalate as backsheet. A separation and recovery of these materials was possible using the theory of solvent dissolution of Hildebrand, comprising thermodynamics and kinetics. The separation occurred in 24h at 860rpm, rising the modules in isopropyl alcohol and potentially reaching 6h at 860rpm when rising them in tetrahydrofuran. The silver leaching from the semiconductor phase was possible in sulphuric acid 4 mol.L-1, 95°C, under addition of 6mL of hydrogen peroxide every 15min, reaching 100% silver leached in 2h. Shifting the temperature to 30°C, the leaching would occur completely only after 6h of experiment. The silver was precipitated as a chloride from the solution by addition of sodium chloride. The amorphous silicon module showed that EVA was present in the polymeric phase and silicon, germanium, silver, tin and indium (the last one at concentration of 0,34g/m2 in area of the module) in the metallic phase, observed on the micrographies and chemical analyses. Calcination was performed at 400°C, removing the EVA and freeing the silver contacts. Indium was 100% leached with a 1mol.L-1 phosphoric acid solution at 75°C, under 800rpm and solid-liquid ratio of 1g.10mL-1 in 1h.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2019-02-01
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.