Disertación de Maestría
DOI
https://doi.org/10.11606/D.3.2010.tde-20082010-134833
Documento
Autor
Nombre completo
Erick Batista Rodrigues
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Paulo, 2010
Director
Tribunal
Wang, Shu Hui (Presidente)
Costa, Argemiro Luís de Aragão
Valenzuela Díaz, Francisco Rolando
Título en portugués
Estudo da estabilidade das propriedades mecânicas e químicas de compostos de borracha vulcanizados com enxofre após envelhecimento térmico e oxidativo.
Palabras clave en portugués
Borracha natural
Elastômero
Envelhecimento
Estabildiade
Vulcanização
Resumen en portugués
O aumento da vida útil de pneus tem sido uma incessante busca de seus fabricantes. Aumentar a vida de um pneu não significa somente prolongar sua vida, mas também manter estáveis as características e propriedades, para as quais os compostos foram projetados. Para manter estáveis as propriedades e características dos compostos, deve-se ter a estabilidade das ligações cruzadas formadas durante a vulcanização do pneu. Em condições normais de uso, os principais causadores da degradação das ligações cruzadas em compostos de pneus são os ataques térmicos e oxidativos. O objetivo deste trabalho é avaliar a estabilidade de um composto de borracha natural frente às solicitações térmica e oxidativa das ligações cruzadas formadas sob diferentes condições de vulcanização e sistemas vulcanizantes. Foram elaboradas cinco formulações baseadas em borracha natural do tipo RSS-3 e com variações na dosagem de enxofre e óxido de zinco, utilizando sistemas de vulcanização convencional e eficiente. Todos os compostos foram vulcanizados em duas condições, 170°C e 140°C. Os compostos vulcanizados foram avaliados em ensaios físicos e químicos, incluindo medições de módulos de armazenamento e de perda, tensão e alongamentos à ruptura, resistência à laceração, densidade de ligações cruzadas e cinética de vulcanização nas condições novo (original) e envelhecidos na presença e na ausência de oxigênio. Os resultados obtidos permitem afirmar que a utilização de oxido de zinco de alta área superficial e de sistemas de vulcanização eficientes tornam este tipo de composto mais resistentes ao envelhecimento térmico e oxidativo.
Título en inglés
Study of stability of the mechanical and chemical properties of rubber compunds vulcanized with sulfur after heat and oxidative aging.
Palabras clave en inglés
Aging
Curing
Elastomer
Natural rubber
Zinc oxide
Resumen en inglés
The increment of the service life of tires has been a constant challenge for their manufacturers. Increasing the life of a tire does not mean only prolong his life, but also maintain its characteristics and properties stable, whatever the compounds were designed for. To keep stable the properties and characteristics of the compounds, we must have the stability of the crosslinks formed during the vulcanization of the tire. In normal use, the main causes of the degradation of the crosslinks are due to the thermal and oxidative attacks. The objective of this study is to evaluate the thermal and oxidative stability of the crosslinks formed under different conditions and curing systems in a compound with natural rubber. Five formulations were prepared based on the natural rubber RSS-3 and variations in the dosage of sulfur and zinc oxide, as well as the type of the vulcanization system, conventional or efficient, were introduced. All compounds were cured in two conditions, 170°C and 140°C. The vulcanized compounds were evaluated by physical and chemical tests, including measurements of the storage and loss moduli, tension and stretching to break, tear resistance, crosslinking density and kinetics of curing. The performance of the compounds was evaluated under three conditions, namely new (original) and after aging in the presence and in the absence of oxygen. The results allowed us to conclude that the use of zinc oxide of high surface area and the efficient vulcanization systems are more resistant to thermal and oxidative aging.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2010-09-16
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.