Nom complet
Flávio Gil Alves Paiva
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Paulo, 2009
Directeur
Jury
Brandi, Sérgio Duarte (Président)
Azevedo, César Roberto de Farias
Souza, Paulo Cezar Rioli Duarte de
Titre en portugais
Caracterização de junta soldada por atrito linear com mistura (FSW) da liga Al-Mg-Si AA 6063.
Mots-clés en portugais
Alumínio
Soldagem no estado sólido
Soldagem por atrito linear com mistura
Resumé en portugais
O processo de soldagem por atrito linear com mistura (SALM), ou Friction Stir Welding, surgiu do desejo de se aplicar os princípios e vantagens da soldagem em estado sólido do processo por atrito tradicional em outras geometrias que não fossem axi-simétricas. Assim, foi acrescentada uma velocidade de translação e uma ferramenta rotativa especial, sendo possível realizar cordões de solda em ligas antes com soldabilidade bem ruim. O fator chave para se ter uma solda por atrito linear com mistura sã é a combinação correta entre o a geometria da ferramenta, os parâmetros de soldagem e o fluxo de material durante a soldagem. O lado do avanço, em relação à velocidade de translação da ferramenta, está sob tração, enquanto que o lado do retrocesso está sob compressão. Cada um destes lados possui características diferenciadas, tanto microestruturais como de propriedades mecânicas. O objetivo deste trabalho é caracterizar o cordão de solda feito em liga AA6063T6 com 3 mm de espessura. O material foi soldado com uma ferramenta tipo Three flats, com rotação de 1120 rpm e velocidade de soldagem de 5,3 mm/s. Os corpos de prova foram caracterizados por microscopia óptica, microdureza e ensaio de tração. Os resultados mostraram que o cordão de solda é assimétrico, sendo 20% maior do lado do avanço da ferramenta. Além disto, houve um refino de grão e, na transição entre a zona termomecanicamente afetada (ZTMA) e a zona afetada pelo calor (ZAC), os grãos alongados apresentaram fator de forma maior no lado do avanço (entre 1,73 e 2,74) do que no lado do retrocesso (entre 1,40 e 1,59). As extensões da zona termomecanicamente afetada e da zona afetada pelo calor são maiores do lado do avanço que do lado do retrocesso.
Titre en anglais
Friction stir welded joint characterization of 6063 aluminum alloy.
Mots-clés en anglais
Aluminium
Friction stir welding
Solid state welding
Resumé en anglais
Friction Stir Welding process arose from a desire to apply the principles and benefits of traditional solid state friction welding friction in non axi-symmetric geometries. Thus, it was added a traveling speed and a special rotating tool that allows welding aluminum alloys with bad weldability. The key factor to have a linear friction welding with sound bead is a combination of tool geometry, welding parameters and material flow during welding, which is under tension stress in the advancing side and in compression in the retrieving side. Thus, each side has different microstructures and mechanical properties. The objective of this work is to characterize the 3,0 mm weld bead of an alloy 6063 T6. This material was welded with a tool type "Three flats" with a rotation speed of 1120 rpm and welding traveling speed of 5.3 mm/s. The samples were characterized by optical microscopy, microhardness testing and tensile test. The results showed that the weld bead is asymmetric, with an area 20% higher in the advancing side. Moreover, a grain refining process occurred in the weld bead and, in the transition region between thermomechanically affected zone (TMAZ) and heat affected zone (HAZ) the elongated grains presented a shape factor higher in the advancing side (1,73 to 2,74) than in the retrieving side (1,40 to 1,59). Also, the thermomechanically affected zone and the heat affected zone presented a larger width in the advancing side than in the retrieving side.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2010-09-28
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.