• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Master's Dissertation
DOI
https://doi.org/10.11606/D.25.1996.tde-06042005-094511
Document
Author
Full name
Renata Bastos Del'Hoyo Fernandes
Institute/School/College
Knowledge Area
Date of Defense
Published
Bauru, 1995
Supervisor
Committee
Navarro, Maria Fidela de Lima (President)
Carvalho, Ricardo Marins de
Taga, Eulazio Mikio
Title in Portuguese
Avaliação in vitro da liberação de flúor de cimentos de ionômero de vidro forradores e cimentantes.
Keywords in Portuguese
dentística
materiais dentários
Abstract in Portuguese
O objetivo deste estudo in vitro foi avaliar e comparar o padrão e a quantidade de liberação de flúor de cimentos de ionômero de vidro forradores e cimentantes após períodos de 24 horas, 7 dias e 28 dias em água desionizada. Foram confeccionados 6 corpos de prova em forma de disco para cada material e cada período de leitura que, após a reação de endurecimento inicial, foram suspensos em recipientes plásticos contendo 18 mL de água desionizada. No momento da leitura, realizada a cada 6 horas no período de 24 horas, a cada 24 horas no período de 7 dias e a cada 7 dias no período de 28 dias, adicionou-se ao meio de armazenagem 2 mL de solução tampão TISAB III. A concentração de íons flúor em solução foi avaliada mediante leitura potenciométrica utilizando-se um aparelho analisador de íons. Vidrion C e XR Ionomer apresentaram as maiores quantidades de liberação de flúor. Ketac-Bond, Vitrebond, Ketac-Cem, GC Fuji I e Shofu I ocuparam uma posição intermediária e o Zionomer pó/líquido liberou a menor quantidade de flúor. Contudo, o padrão de liberação de flúor foi semelhante para todos os materiais testados.
Abstract in English
The objective of the present in vitro study was to evaluate and compare the pattern and the quantity of fluoride release of lining and luting glass ionomer cements after 24 hours, 7 days and 28 days in de-ionized water. Six disc-shaped specimes were made for each material and for each reading period. After the initial hardening reaction, they were pierced and suspended in plastic containers with 18 mL of de-ionized water. Readings were carried out every six hours in the 24-hour period, every 24 hours in the 7- day period, and every 7 days in the 28-day period, when 2 mL of TISAB III buffer solution was added. The concentration of fluoride ions in solution was evaluated through potenciometric readings using an ion analyser device. Vidrion C and XR Ionomer showed the highest quantity of fluoride release. Ketac-Bond, Vitrebond, Ketac-Cem, GC Fuji I and Shofu I were intermediary in rank, whereas powder/liquid Zionomer released the least quantity of fluoride. However, the pattern of fluoride release was the same to all the tested materials.
 
WARNING - Viewing this document is conditioned on your acceptance of the following terms of use:
This document is only for private use for research and teaching activities. Reproduction for commercial use is forbidden. This rights cover the whole data about this document as well as its contents. Any uses or copies of this document in whole or in part must include the author's name.
Renata.pdf (942.00 Kbytes)
Publishing Date
2005-04-07
 
WARNING: Learn what derived works are clicking here.
All rights of the thesis/dissertation are from the authors
CeTI-SC/STI
Digital Library of Theses and Dissertations of USP. Copyright © 2001-2024. All rights reserved.