Thèse de Doctorat
DOI
https://doi.org/10.11606/T.23.2008.tde-21012009-143919
Document
Auteur
Nom complet
Bruno Lopes da Silveira
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Paulo, 2008
Directeur
Jury
Eduardo, Carlos de Paula (Président)
Aranha, Ana Cecilia Corrêa
Francischone, Carlos Eduardo
Soares, Sheila Cynthia Gouw
Valandro, Luiz Felipe
Titre en portugais
Avaliação in vitro da resistência adesiva e degradação da interface de união entre cimentos resinosos e uma cerâmica aluminizada tratada internamente com laser
Mots-clés en portugais
Cerâmica
Hipoclorito de sódio
Laser de Nd:YAG
Microtração
Óxido de alumínio
Rocatec
Resumé en portugais
O estudo teve o objetivo de avaliar a resistência adesiva e a degradação da interface entre uma cerâmica tratada com laser e cimentos resinosos. Sessenta e quatro blocos cerâmicos foram distribuídos em 16 grupos distribuídos de acordo com os fatores em estudo: tratamento da superfície interna da cerâmica: Oxido de Alumínio (Ox), Rocatec (R), Laser de Nd:YAG 141,54 J/cm2 (Nd) e Laser de Nd:YAG + Rocatec (NdR); cimentos resinosos: Panavia F (Kuraray) e Relyx Unicem (3M ESPE); e método de envelhecimento: água destilada (W) e hipoclorito de sódio 10% (H). Após os procedimentos de cimentação e corte dos blocos, metade dos palitos foi armazenada em solução de hipoclorito de sódio 10% para simular envelhecimento in vitro. A resistência de união foi avaliada através do ensaio de microtração (0,5 mm/min) e os padrões de fratura foram classificados em adesivo, coesivo ou misto. Blocos cerâmicos adionciais foram confeccionados e analisados em Microscopia Eletrônica de Varredura e em Microscópio de Força Atômica para verificação dos padrões gerados pelos tratamentos. Os grupos tratados com laser de Nd:YAG apresentaram os maiores valores de resistência de união. Para os grupos cimentados com Panavia F, os valores de resistência de união foram: OxW: 27,71±6,3; RW: 35,67±5,13; NdW: 42,49±6,8; NdRW: 37,41±4,76; OxH: 22,27±6,05; RH: 27,49±8,83; NdH: 32,24±6,94; NdRH: 31,75±7,77. Para os grupos com RelyX Unicem: OxW: 26,74±6,34; RW: 35,07±6,02; NdW: 41,05±7,71; NdRW: 33,85±6,03; OxH: 22,77±7,37; RH: 27,84±6,26; NdH: 36,42±5,08; NdRH: 27,6±5,8. Pode-se concluir que o laser de Nd:YAG foi o tratamento mais efetivo, seguido da associação entre o laser de Nd:YAG+Rocatec, Rocatec e jateamento com Al2O3. Os cimentos testados apresentam comportamentos similares. O envelhecimento in vitro com hipoclorito de sódio diminuiu os valores de resistência de união.
Titre en anglais
In Vitro analsis of bond strength and degradation method between bond interface of aluminous ceramic and resin cements
Mots-clés en anglais
Aluminum oxide sandblasting
Ceramic
Microtensile test
Nd:YAG laser
Rocatec
Sodium hypochlorite
Resumé en anglais
The aim of this study was to evaluate the influence of different surface treatments on resistance to degradation between In-Ceram Alumina and two resin-based cements. Sixteen experimental groups were formed according to ceramic treatment: Sandblasting (S), Rocatec System (R), Nd:YAG Laser (Nd), Nd:YAG Laser plus Rocatec System (NR); luting cement: Panavia F (Kuraray) or Relyx Unicem (3M ESPE); and aging method: water (W) or sodium hypochlorite (H). Sixty four In-Ceram Alumina blocks (10x10x6mm) received four surface treatments: Al2O3 sandblasting; Al2O3 sandblasting + Rocatec Plus; Al2O3 sandblasting + Nd:YAG Lase; Al2O3 sandblasting + Nd:YAG Laser + Rocatec Plus. Each conditioned ceramic block was bonded to a composite block using a resin cement system. After 24h storage time, the blocks were sectioned to obtain sticks with cross-sectional area of 1.0mm2. The specimens were loaded to failure in a universal testing machine at a crosshead speed of 0.5mm/min. The fractured surface morphology of the debonded specimens was observed (40X) to evaluate the fracture pattern. Failure modes were classified as adhesive, cohesive in ceramic, cohesive in resin cement and mixed. The ceramic treatment and the aging method significantly affected the microtensile bond strength. Nd:YAG surface treatment resulted in the best bond strength values. To groups luted with Panavia F cement the microtensile bond strength values were: SW: 27,71±6,3; RW: 35,67±5,13; NdW: 42,49±6,8; NdRW: 37,41±4,76; SH: 22,27±6,05; RH: 27,49±8,83; NdH: 32,24±6,94; NdRH: 31,75±7,77. To groups luted with RelyX cement: SW: 26,74±6,34; RW: 35,07±6,02; NdW: 41,05±7,71; NdRW: 33,85±6,03; SH: 22,77±7,37; RH: 27,84±6,26; NdH: 36,42±5,08; NdRH: 27,6±5,8. Nd:YAG laser was the most effective surface treatment, followed by Nd:YAG+Rocatec, Rocatec and Al2O3 sandblasting. Resin cements presented similar behaviors in spite of aging. NaOCl 12h-immersion decreased Bond strength values.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2009-03-16
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.