Tesis Doctoral
DOI
https://doi.org/10.11606/T.23.2007.tde-11042008-105741
Documento
Autor
Nombre completo
Ninoshka Uceda Gómez
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Paulo, 2007
Director
Tribunal
Oda, Margareth (Presidente)
Bocangel, Jorge Antonio Javier Saldivar
Kenshima, Silvia
Silva, Alessandra Reis
Vieira, Glauco Fioranelli
Título en portugués
Degradação de interfaces adesivas formadas após desmineralização e desproteinização da dentina
Palabras clave en portugués
Dentina
Hipoclorito de sódio
Microtração
Resistência de união
Sistemas adesivos
Resumen en portugués
O objetivo deste estudo foi avaliar a resistência de união de 2 sistemas adesivos convencionais de dois passos (Single Bond-SB, 3MESPE e One Step-OS, Bisco) aplicados à dentina desmineralizada [SH] e desmineralizada e desproteinizada com NaOCl a 10% [CH], tanto no tempo imediato [IM] como após 12 meses de imersão em água [12M]. Realizou-se também a observação da morfologia das interfaces de união entre os sistemas adesivos e a superfície de dentina em Microscópio Eletrônico de Varredura (MEV) para cada grupo experimental. O esmalte oclusal de 20 molares permanentes hígidos foi removido para expor as superfícies planas de dentina, que foram condicionadas com H3PO4 a 37%, lavadas e secas (grupos SH). Para os grupos CH após o condicionamento ácido foi aplicado hipoclorito de sódio a 10% durante 60 s, seguido de lavagem por 15 s. Os sistemas adesivos foram aplicados de acordo com as recomendações dos fabricantes. Coroas de resina composta (Z-250, 3MESPE) foram construídas de forma incremental (600 mW/cm² por 40 s). Após armazenagem em água por 24h a 37°C, os espécimes foram secionados para obter corpos-de-prova na forma de palitos (0,8mm²), que foram testados sob tração (0,5 mm/min) no tempo imediato [IM] ou após 12 meses de armazenamento em água. Dois dentes de cada grupo foram observados em MEV nos dois períodos de tempo. Os dados de resistência de união foram submetidos à uma análise de variância de três fatores e teste de Tukey para contraste das médias (p = 0,05). As interações duplas e triplas não foram estatisticamente significantes (p> 0,05), assim como o fator principal Tratamento de superfície (p = 0,05). Somente os fatores principais Adesivo e Tempo de armazenagem foram significantes (p = 0,04 e p = 0,03, respectivamente). O adesivo SB (43,3 ± 9,1 MPa) apresentou altos valores de resistência de união quando comparado com o OS (33,3 ± 11,6 MPa). A resistência de união do grupo IM (42,5 ± 8,7) foi estatisticamente superior à grupo 12M (33,3 ± 11,8).
Título en inglés
Long-term bond strengths of adhesive systems applied to etched and deproteinized dentin
Palabras clave en inglés
Adhesive systems
Dentin
Micro-tensile bond strength
Sodium Hypochlorite
Resumen en inglés
The aim of this study was to evaluate the early and 12-month bond strengths of two adhesive systems (Single Bond-SB, 3MESPE and One Step-OS, Bisco) applied to demineralized dentin (WH) and demineralized/NaOCl-treated dentin (H). The adhesive interfaces were also micromorphologically evaluated by Scanning Electron Microscopy (SEM). Twenty flat dentin surfaces were exposed. They were etched, rinsed and slightly dried. For the H groups, a solution of 10% NaOCl was applied for 60s, rinsed (15 s) and slightly dried. The adhesives were applied according to the manufacturer's instructions and composite resin crowns were incrementally constructed. After 24 h (water-37°C), the sample was sectioned in order to obtain resin-dentin sticks (0.8 mm²). The specimens were tested in tension (0.5 mm/min) immediately (IM) or after 12 months of water storage (12M). Two teeth from each experimental group were restored as described previously and evaluated under SEM, under the two storage periods. The data (MPa) were subjected to three-way ANOVA and Tukey's test (? = 0.05). No significant effects for the triple and double interactions (p > 0.05) as well as for the main factor Surface treatment were observed (p > 0.05). Only the main factors Adhesive and Storage time were statistically significant (p = 0.004 and p = 0.003, respectively). The adhesive SB (42.3 ± 9.1) showed higher bond strengths than OS (33.6 ± 11.6). The mean bond strength for IM-group (42.5 ± 8.7) was statistically superior to 12M (33.3 ± 11.8). The use of 10% sodium hypochlorite, after acid etching, did not improve the immediate and the long term resin-dentin bond strengths for acetone and water/alcohol based adhesive systems.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2008-06-09
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.