• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.18.2015.tde-27052015-172300
Documento
Autor
Nombre completo
Jackson Deliz Ditz
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
São Carlos, 2015
Director
Tribunal
El Debs, Mounir Khalil (Presidente)
Carrazedo, Ricardo
Siqueira, Gustavo Henrique
Título en portugués
Desempenho de almofadas de argamassa modificada na transferência de tensões de compressão em ligações de concreto pré-moldado
Palabras clave en portugués
Almofada de apoio
Almofada de argamassa
Ligações de concreto pré-moldado à compressão
Resumen en portugués
Esta pesquisa visa analisar a transferência de tensões de compressão entre elementos de concreto pré-moldado através de almofadas de argamassa modificada. A argamassa foi modificada com as adições de fibras de polipropileno, látex estireno-butadieno e vermiculita termo-expandida. A caracterização da argamassa foi realizada com ensaios de compressão, de tração por compressão diametral e de módulo de elasticidade, além de ensaios de rigidez de almofada, que medem a capacidade da peça de se deformar sob tensão de compressão uniforme. As análises de transferência de tensões foram realizadas intercalando uma almofada entre dois blocos de concreto e submetendo o corpo de prova formado a ensaios de compressão. Os parâmetros variados nesses ensaios foram: rugosidade superficial e resistência mecânica dos blocos ligados, excentricidade de carregamento, solidarização ou não da almofada ao bloco inferior de concreto e carregamento monotônico e cíclico. Em relação à massa do cimento, a argamassa das almofadas possuía 30% de agregados, dos quais 95% eram areia fina e 5% eram vermiculita, 10% de látex, 2% de taxa volumétrica de fibras de polipropileno e relação água / cimento de 0,25, além da água incorporada no látex. A argamassa apresentou resistência à compressão média de 27,65 MPa, resistência à tração de 3,62 MPa e módulo de elasticidade igual a 11,53 GPa. Os principais resultados dos ensaios de ligação foram: a) para compressão centrada, a presença da almofada aumentou a resistência em 20% para espessuras de saliências de 0,5 mm e 30% para saliências de 1,0 mm; b) ganho de efetividade da almofada à medida que se reduziu a resistência do concreto; c) em ligações excêntricas, a dispersão dos resultados não permitiu uma correta avaliação dos resultados; d) para carregamento cíclico, a almofada de apoio aumentou em 45% a resistência da ligação.
Título en inglés
Performance of modified mortar pads in the compression stresses transfer in precast concrete connections
Palabras clave en inglés
Bearing pad
Mortar pad
Precast concrete compressive connections
Resumen en inglés
This research aims to analyze the compressive stresses transfer between precast concrete elements by modified mortar pads. The mortar was modified with additions of polypropylene fibers, styrene-butadiene latex and heat-expanded vermiculite. Mortar characterization was performed in compression, tension and elastic modulus tests, further pad rigidity tests, that measure the pad capacity to deform under uniform compressive stress. Stress transfer analyzes were performed interleaving a bearing pad between two concrete blocks and subjecting the specimen formed in the compression tests. Varied parameters in these tests were: surface roughness and mechanical strength of the connected blocks, loading eccentricity, solidarization or not of the bearing pad to the bottom concrete block and monotonic and cyclic loading. In relation to the cement weight, the mortar of the pads showed 30% of aggregates, which 95% were fine sand and 5% were vermiculite, 10% of latex, 2% of volumetric rate of polypropylene fibers and water / cement ratio of 0,25, in addition of water incorporated into the latex. The mortar showed compression strength of 27,65 MPa, tension strength of 3,62 MPa and elastic modulus equal to 11,53 GPa. The main results of connection test were: a) for centered compression, presence of pad increased the strength in 20% for thicknesses of imperfections of 0,5 mm and 30% for imperfections of 1,0 mm; b) gain of effectiveness of the bearing pad when the concrete strength was reduced; c) in eccentrical connections, the dispersion of results did not allowed a correct evaluation of results; d) for cyclic loading, the bearing pad increased in 45% the connections strength.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2015-05-29
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.